Ti50.75Ni47.75Fe1.50 |
|
Sitepu H, Wright J P, Hansen T, Chateigner D, Brokmeier H G, Ritter C, Ohba T |
|
Materials Science Forum 495 (2005) 255-260 |
|
Combined synchrotron and neutron structural refinement of R-phase in |
|
Ti50.75Ni47.75Fe1.50 shape memory alloy |
|
_database_code_amcsd 0014391 |
|
4.2579 4.2579 5.2149 90 90 120 P3 |
|
atom x y z occ Uiso |
|
Ti1 0 0 0 .875 .00714 |
|
Ni2 0 0 .5249 .00587 |
|
Ti3 -.0129 .3248 .6463 .875 .00714 |
|
Ni4 -.0116 .3364 .1306 .00587 |
|
Ti5 1/3 2/3 .0150 .875 .00714 |
|
Ni6 1/3 2/3 .5301 .00587 |
|
Ti7 .0063 .6748 .3314 .875 .00714 |
|
Ni8 .0204 .6834 .8336 .00587 |
|
Ti9 2/3 1/3 -.0447 .875 .00714 |
|
Ni10 2/3 1/3 .4172 .00587 |
|
|