Brucite
      Nagai T, Hattori T, Yamanaka T
      American Mineralogist 85 (2000) 760-764
      Compression mechanism of brucite: An investigation by the structural refinement
      under pressure
      Sample: P = 16.0 GPa
      _database_code_amcsd 0002437

      CELL PARAMETERS:    3.0003   3.0003   4.3250   90.000   90.000  120.000
      SPACE GROUP: P-3m1     
      X-RAY WAVELENGTH:     1.541838
      Cell Volume:     33.717
      Density (g/cm3):      2.773
      MAX. ABS. INTENSITY / VOLUME**2:      20.29462403    
      RIR:      2.383
      RIR based on corundum from Acta Crystallographica A38 (1982) 733-739
               2-THETA      INTENSITY    D-SPACING   H   K   L   Multiplicity
                20.54         56.16        4.3250    0   0   1         2
                34.52          4.78        2.5983    1   0   0         6
                40.50         99.85        2.2273    0   1   1         6
                55.27         21.76        1.6622    0   1   2         6
                55.27         19.26        1.6622    1   0   2         6
                61.85         23.77        1.5001    1   1   0         6
                64.65          1.41        1.4417    0   0   3         2
                65.90          9.68        1.4173    1   1   1        12
                75.40          9.67        1.2606    1   0   3         6
                76.57          8.67        1.2442    2   0   1         6
                87.62          3.80        1.1136    2   0   2         6
                87.62          3.41        1.1136    0   2   2         6
================================================================================
       XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs