(K.4Na.6)Cl
      Walker D, Verma P K, Cranswick L M D, Jones R L, Clark S M, Buhre S
      American Mineralogist 89 (2004) 204-210
      Halite-sylvite thermoelasticity
      Sample: r57196, T = 650 C, P = 25.2 kbar, cell volume = 200.74 ang**3
      _database_code_amcsd 0003338

      CELL PARAMETERS:    5.8552   5.8552   5.8552   90.000   90.000   90.000
      SPACE GROUP: Fm3m      
      X-RAY WAVELENGTH:     1.541838
      Cell Volume:    200.736
      Density (g/cm3):      2.147
      MAX. ABS. INTENSITY / VOLUME**2:      33.24760947    
      RIR:      5.043
      RIR based on corundum from Acta Crystallographica A38 (1982) 733-739
               2-THETA      INTENSITY    D-SPACING   H   K   L   Multiplicity
                26.36          1.63        3.3805    1   1   1         8
                30.54        100.00        2.9276    2   0   0         6
                43.73         61.65        2.0701    2   2   0        12
                54.27         18.58        1.6903    2   2   2         8
                63.56          7.61        1.4638    4   0   0         6
                72.15         18.90        1.3093    4   2   0        24
                80.33         12.98        1.1952    4   2   2        24
================================================================================
       XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs