Metatorbernite
Stubbs J E, Post J E, Elbert D C, Heaney P J, Veblen D R
American Mineralogist 95 (2010) 1132-1140
Uranyl phosphate sheet reconstruction during dehydration of
metatorbernite [Cu(UO2)2(PO4)2*8H2O]
Note: This is the 8.7 Angstrom phase while heating at 31.5 C
Locality: Bois Noirs, France
_database_code_amcsd 0016811
6.96519 6.96519 17.3102 90 90 90 *P4/n
.25 -.25 0
atom     x     y      z  Uiso
Cu     .25   .25  .3092 .0072
U1     .25   .25 .05242 .0083
U2     .25   .25 .55092 .0083
P1     .25   .75      0 .0138
P2     .25   .75     .5 .0138
O1     .25   .25  .4474   .01
O2     .25   .25  .9484   .01
O3     .25   .25  .6521   .01
O4     .25   .25  .1542   .01
O5    .299 .9083  .0571   .01
O6    .215 .9304  .5482   .01
Wat7 .5280 .2797  .3147   .01
Wat8 .3392 .5149  .8048   .01