Metatorbernite
Stubbs J E, Post J E, Elbert D C, Heaney P J, Veblen D R
American Mineralogist 95 (2010) 1132-1140
Uranyl phosphate sheet reconstruction during dehydration of
metatorbernite [Cu(UO2)2(PO4)2*8H2O]
Note: This is the 6.9 Angstrom phase while heating at 173 C
Locality: Bois Noirs, France
_database_code_amcsd 0016813
14.4979 7.0159 6.6312 90 107.585 90 P2_1
atom       x     y     z  occ  Uiso
Cu1    .2324  .475  .527 .930  .008
U1     .0188 .7894 .1541      .0114
U2     .4942 .2192 .8375      .0114
P1     .0559 .2993 .3491       .027
P2     .4918 .7013 .6356       .027
O1     .1461  .844  .227        .01
O2     .3627  .245  .774        .01
O3    -.1081  .730  .086        .01
O4     .6234  .206  .889        .01
O5     .0542  .469  .202        .01
O6     .5189  .539  .801        .01
O7     .0130  .125  .202        .01
O8     .5060  .884  .773        .01
O9    -.0110  .339  .491        .01
O10    .5654  .703  .519        .01
O11    .1596  .250  .472        .01
O12    .3844  .689  .497        .01
Wat13   .749 -.041  .042        .01
Wat14   .701 -.191  .724        .01
Wat15   .731  .499  .792        .01