Monteponite
      Zhang J
      Physics and Chemistry of Minerals 26 (1999) 644-648
      Room temperature compressibilities of MnO and CdO: further
      examination of the role of cation type in bulk modulus systematics
      Sample from Run #1: P = 6.17 GPa
      _database_code_amcsd 0008262

      CELL PARAMETERS:    4.6366   4.6366   4.6366   90.000   90.000   90.000
      SPACE GROUP: Fm3m      
      X-RAY WAVELENGTH:     1.541838
      Cell Volume:     99.678
      Density (g/cm3):      8.556
      MAX. ABS. INTENSITY / VOLUME**2:      294.3587087    
      RIR:     11.203
      RIR based on corundum from Acta Crystallographica A38 (1982) 733-739
               2-THETA      INTENSITY    D-SPACING   H   K   L   Multiplicity
                33.47        100.00        2.6769    1   1   1         8
                38.85         86.63        2.3183    2   0   0         6
                56.10         50.14        1.6393    2   2   0        12
                66.93         33.59        1.3980    3   1   1        24
                70.34         14.69        1.3385    2   2   2         8
                83.38          6.23        1.1592    4   0   0         6
================================================================================
       XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs