Avicennite
      Otto H H, Baltrusch R, Brant H J
      Physica C 215 (1993) 205-208
      Further evidence for Tl3+ in Tl-based superconductors from improved
      bond strength parameters involving new structural data of cubic Tl2O3
      _database_code_amcsd 0015057

      CELL PARAMETERS:   10.5344  10.5344  10.5344   90.000   90.000   90.000
      SPACE GROUP: Ia3       
      X-RAY WAVELENGTH:     1.541838
      Cell Volume:   1169.040
      Density (g/cm3):     10.379
      MAX. ABS. INTENSITY / VOLUME**2:      743.2588254    
      RIR:     23.317
      RIR based on corundum from Acta Crystallographica A38 (1982) 733-739
               2-THETA      INTENSITY    D-SPACING   H   K   L   Multiplicity
                20.65          8.98        4.3007    2   1   1        24
                29.37        100.00        3.0410    2   2   2         8
                31.78          1.06        2.8154    3   2   1        24
                31.78          1.45        2.8154    3   1   2        24
                34.04         38.31        2.6336    4   0   0         6
                36.18          5.53        2.4830    4   1   1        24
                40.15          2.84        2.2459    3   3   2        24
                43.82          3.75        2.0660    4   3   1        24
                43.82          4.07        2.0660    4   1   3        24
                47.26          1.02        1.9233    5   2   1        24
                47.26          1.09        1.9233    5   1   2        24
                48.91         34.24        1.8622    4   4   0        12
                50.52          2.30        1.8066    4   3   3        24
                53.63          3.39        1.7089    6   1   1        24
                56.62          1.96        1.6255    5   1   4        24
                56.62          1.75        1.6255    5   4   1        24
                58.08         29.70        1.5881    6   2   2        24
                59.52          2.59        1.5532    6   3   1        24
                59.52          2.69        1.5532    6   1   3        24
                60.93          6.79        1.5205    4   4   4         8
                62.33          1.22        1.4898    5   4   3        24
                62.33          1.02        1.4898    5   3   4        24
                65.06          1.50        1.4336    6   3   3        24
                66.41          1.23        1.4077    6   4   2        24
                70.37          1.24        1.3379    6   5   1        24
                70.37          1.29        1.3379    6   1   5        24
                71.67          3.64        1.3168    8   0   0         6
                72.96          1.56        1.2967    8   1   1        24
                75.51          1.13        1.2591    6   5   3        24
                75.51          1.12        1.2591    6   3   5        24
                76.77          1.16        1.2415    8   2   2        24
                78.03          1.10        1.2246    8   1   3        24
                78.03          1.17        1.2246    8   3   1        24
                79.28          7.66        1.2084    6   6   2        24
                81.77          3.20        1.1778    8   0   4        12
                81.77          3.20        1.1778    8   4   0        12
                83.01          1.01        1.1633    8   3   3        24
================================================================================
       XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs
  For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.