Cobalt
      Marick L
      Physical Review 49 (1936) 831-837
      Variation of resistance and structure of cobalt with temperature
      and a discussion of its photoelectric emission
      Locality: synthetic
      Sample: at T = 295 C
      Note: photograph 3
      _database_code_amcsd 0015137

      CELL PARAMETERS:    2.5270   2.5270   4.1190   90.000   90.000  120.000
      SPACE GROUP: P6_3/mmc  
      X-RAY WAVELENGTH:     1.541838
      Cell Volume:     22.779
      Density (g/cm3):      8.591
      MAX. ABS. INTENSITY / VOLUME**2:      230.8690436    
      RIR:      8.750
      RIR based on corundum from Acta Crystallographica A38 (1982) 733-739
               2-THETA      INTENSITY    D-SPACING   H   K   L   Multiplicity
                41.25         25.36        2.1884    1   0   0         6
                43.97         27.65        2.0595    0   0   2         2
                47.02        100.00        1.9326    1   0   1        12
                61.86         12.83        1.4998    1   0   2        12
                75.20         12.74        1.2635    1   1   0         6
                83.03         13.79        1.1631    1   0   3        12
                89.58          1.85        1.0942    2   0   0         6
================================================================================
       XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs
  For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.