Cobalt
      Marick L
      Physical Review 49 (1936) 831-837
      Variation of resistance and structure of cobalt with temperature
      and a discussion of its photoelectric emission
      Locality: synthetic
      Sample: at T = 420 C
      Note: photograph 4
      _database_code_amcsd 0015138

      CELL PARAMETERS:    2.5360   2.5360   4.1360   90.000   90.000  120.000
      SPACE GROUP: P6_3/mmc  
      X-RAY WAVELENGTH:     1.541838
      Cell Volume:     23.036
      Density (g/cm3):      8.495
      MAX. ABS. INTENSITY / VOLUME**2:      228.6644574    
      RIR:      8.765
      RIR based on corundum from Acta Crystallographica A38 (1982) 733-739
               2-THETA      INTENSITY    D-SPACING   H   K   L   Multiplicity
                41.10         25.33        2.1962    1   0   0         6
                43.77         27.68        2.0680    0   0   2         2
                46.84        100.00        1.9397    1   0   1        12
                61.60         12.86        1.5056    1   0   2        12
                74.89         12.76        1.2680    1   1   0         6
                82.63         13.82        1.1677    1   0   3        12
                89.18          1.85        1.0981    2   0   0         6
================================================================================
       XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs
  For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.