Cobalt
      Marick L
      Physical Review 49 (1936) 831-837
      Variation of resistance and structure of cobalt with temperature
      and a discussion of its photoelectric emission
      Locality: synthetic
      Sample: at T = 843 C
      Note: photograph 12
      _database_code_amcsd 0015143

      CELL PARAMETERS:    3.6020   3.6020   3.6020   90.000   90.000   90.000
      SPACE GROUP: Fm3m      
      X-RAY WAVELENGTH:     1.541838
      Cell Volume:     46.734
      Density (g/cm3):      8.375
      MAX. ABS. INTENSITY / VOLUME**2:      250.6987727    
      RIR:      9.747
      RIR based on corundum from Acta Crystallographica A38 (1982) 733-739
               2-THETA      INTENSITY    D-SPACING   H   K   L   Multiplicity
                43.52        100.00        2.0796    1   1   1         8
                50.69         45.34        1.8010    2   0   0         6
                74.51         23.02        1.2735    2   2   0        12
================================================================================