Grossular Meagher E P American Mineralogist 60 (1975) 218-228 The crystal structures of pyrope and grossularite at elevated temperatures T = 25 deg C garnet _database_code_amcsd 0000450 CELL PARAMETERS: 11.8460 11.8460 11.8460 90.000 90.000 90.000 SPACE GROUP: Ia-3d X-RAY WAVELENGTH: 1.541838 Cell Volume: 1662.322 Density (g/cm3): 3.599 MAX. ABS. INTENSITY / VOLUME**2: 25.64507886 RIR: 2.320 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 30.18 35.78 2.9615 4 0 0 6 33.84 100.00 2.6488 4 2 0 24 35.55 6.70 2.5256 3 3 2 24 37.18 17.97 2.4181 4 2 2 24 38.76 14.21 2.3232 4 3 1 48 41.76 12.96 2.1628 5 2 1 48 43.20 3.25 2.0941 4 4 0 12 47.30 9.98 1.9217 5 3 2 48 47.30 11.40 1.9217 6 1 1 24 48.61 1.40 1.8730 6 2 0 24 53.60 15.15 1.7098 4 4 4 8 55.98 25.52 1.6427 6 4 0 24 57.14 1.21 1.6120 5 5 2 24 58.29 40.37 1.5830 6 4 2 48 62.75 9.59 1.4807 8 0 0 6 63.84 1.66 1.4581 7 4 1 48 71.19 9.42 1.3244 8 4 0 24 73.23 16.43 1.2925 8 4 2 48 75.25 6.53 1.2628 6 6 4 24 76.25 1.02 1.2487 8 5 1 48 80.22 1.88 1.1966 9 4 1 48 80.22 2.03 1.1966 8 5 3 48 83.16 1.87 1.1616 10 2 0 24 89.00 9.43 1.0999 8 6 4 48 89.00 5.58 1.0999 10 4 0 24 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.