Muscovite Guggenheim S, Chang Y H, Koster van Groos A F American Mineralogist 72 (1987) 537-550 Muscovite dehydroxylation: High-temperature studies Sample: T = 20 deg C, from Diamond mine, Keystone, South Dakota _database_code_amcsd 0001076 5.200 9.021 20.07 90 95.71 90 C2/c atom x y z occ B(1,1) B(2,2) B(3,3) B(1,2) B(1,3) B(2,3) K 0 .0982 .25 .93 .0147 .0058 .00099 0 .0003 0 Na 0 .0982 .25 .07 .0147 .0058 .00099 0 .0003 0 Al .2511 .0836 .0001 .915 .0039 .0022 .00047 -.0010 .0001 .00008 Fe .2511 .0836 .0001 .08 .0039 .0022 .00047 -.0010 .0001 .00008 AlT1 .4648 .9294 .13565 .225 .0043 .0018 .00051 -.0004 .0001 .00009 SiT1 .4648 .9294 .13565 .775 .0043 .0018 .00051 -.0004 .0001 .00009 AlT2 .4517 .2584 .13545 .225 .0043 .0021 .00047 -.0003 .0001 -.00009 SiT2 .4517 .2584 .13545 .775 .0043 .0021 .00047 -.0003 .0001 -.00009 O1 .4170 .0926 .1683 .013 .0029 .0008 -.0007 .0005 -.0001 O2 .251 .8112 .1582 .012 .0042 .0010 -.0006 .0000 .0006 O3 .251 .3705 .1690 .010 .0042 .0008 .0026 .0002 -.0001 O4 .4579 .9438 .0536 .003 .0028 .0008 -.0003 -.0001 .0001 O5 .3858 .2528 .0537 .007 .0035 .0008 .0004 .0003 .0002 OH .4565 .5636 .0503 .915 .008 .0037 .0005 -.0011 .0005 -.0002 F .4565 .5636 .0503 .085 .008 .0037 .0005 -.0011 .0005 -.0002