Ulvospinel Bosi F, Halenius U, Skogby H American Mineralogist 94 (2009) 181-189 Crystal chemistry of the magnetite-ulvospinel series Locality: synthetic Note: FeTi80Af _database_code_amcsd 0004828 CELL PARAMETERS: 8.5079 8.5079 8.5079 90.000 90.000 90.000 SPACE GROUP: Fd3m X-RAY WAVELENGTH: 1.541838 Cell Volume: 615.839 Density (g/cm3): 4.864 MAX. ABS. INTENSITY / VOLUME**2: 79.06645839 RIR: 5.293 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 18.06 8.03 4.9120 1 1 1 8 29.70 31.82 3.0080 2 2 0 12 34.98 100.00 2.5652 3 1 1 24 36.59 6.87 2.4560 2 2 2 8 42.50 19.10 2.1270 4 0 0 6 52.71 10.29 1.7367 4 2 2 24 56.18 28.09 1.6373 5 1 1 24 56.18 5.53 1.6373 3 3 3 8 61.67 42.02 1.5040 4 4 0 12 69.93 3.60 1.3452 6 2 0 24 72.91 8.82 1.2974 5 3 3 24 73.89 3.83 1.2826 6 2 2 24 77.77 2.39 1.2280 4 4 4 8 85.39 4.24 1.1369 6 4 2 48 88.21 5.90 1.1076 5 5 3 24 88.21 7.83 1.1076 7 3 1 48 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.