Ulvospinel Bosi F, Halenius U, Skogby H American Mineralogist 94 (2009) 181-189 Crystal chemistry of the magnetite-ulvospinel series Locality: synthetic Note: FeTib1b _database_code_amcsd 0004833 CELL PARAMETERS: 8.5322 8.5322 8.5322 90.000 90.000 90.000 SPACE GROUP: Fd3m X-RAY WAVELENGTH: 1.541838 Cell Volume: 621.131 Density (g/cm3): 4.790 MAX. ABS. INTENSITY / VOLUME**2: 74.93001822 RIR: 5.094 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 18.01 8.46 4.9261 1 1 1 8 29.61 33.23 3.0166 2 2 0 12 34.88 100.00 2.5726 3 1 1 24 36.48 6.62 2.4630 2 2 2 8 42.37 18.66 2.1330 4 0 0 6 52.55 10.29 1.7416 4 2 2 24 56.00 28.78 1.6420 5 1 1 24 56.00 5.14 1.6420 3 3 3 8 61.48 40.97 1.5083 4 4 0 12 69.70 3.46 1.3491 6 2 0 24 72.67 8.54 1.3011 5 3 3 24 73.65 3.77 1.2863 6 2 2 24 77.51 2.21 1.2315 4 4 4 8 85.09 4.15 1.1402 6 4 2 48 87.90 7.12 1.1108 7 3 1 48 87.90 5.71 1.1108 5 5 3 24 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.