Argutite Haines J, Leger J M, Chateau C, Pereira A S Physics and Chemistry of Minerals 27 (2000) 575-582 Structural evolution of rutile-type and CaCl2-type germanium dioxide at high pressure Sample: rutile-type, P = 10.5 GPa _database_code_amcsd 0008436 CELL PARAMETERS: 4.3349 4.3349 2.8424 90.000 90.000 90.000 SPACE GROUP: P4_2/mnm X-RAY WAVELENGTH: 1.541838 Cell Volume: 53.413 Density (g/cm3): 6.505 MAX. ABS. INTENSITY / VOLUME**2: 125.0926335 RIR: 6.261 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 29.13 100.00 3.0652 1 1 0 4 37.85 65.20 2.3770 1 0 1 8 41.67 15.23 2.1674 2 0 0 4 43.42 7.56 2.0842 1 1 1 8 46.86 2.37 1.9386 2 1 0 8 57.55 56.86 1.6016 2 1 1 16 60.40 14.92 1.5326 2 2 0 4 65.70 6.72 1.4212 0 0 2 2 68.44 11.21 1.3708 3 1 0 8 73.44 11.33 1.2894 1 1 2 8 73.53 16.66 1.2881 3 0 1 8 80.88 4.72 1.1885 2 0 2 8 88.25 8.32 1.1073 3 2 1 16 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.