Megawite Zhao J, Ross N L, Angel R J Physics and Chemistry of Minerals 31 (2004) 299-305 Tilting and distortion of CaSnO3 perovskite to 7 GPa determined from single-crystal X-ray diffraction Note: P = 1.50 GPa Locality: synthetic _database_code_amcsd 0018607 CELL PARAMETERS: 5.4952 5.6486 7.8561 90.000 90.000 90.000 SPACE GROUP: Pbnm X-RAY WAVELENGTH: 1.541838 Cell Volume: 243.855 Density (g/cm3): 5.632 MAX. ABS. INTENSITY / VOLUME**2: 122.0659308 RIR: 7.058 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 22.57 47.52 3.9388 1 1 0 4 22.64 22.50 3.9281 0 0 2 2 25.29 1.61 3.5210 1 1 1 8 31.68 25.20 2.8243 0 2 0 2 32.18 100.00 2.7813 1 1 2 8 32.59 22.88 2.7476 2 0 0 2 38.07 1.50 2.3640 1 0 3 4 38.18 1.63 2.3570 2 1 1 8 39.29 3.63 2.2931 0 2 2 4 40.05 3.83 2.2515 2 0 2 4 41.40 1.35 2.1807 1 1 3 8 46.09 26.42 1.9694 2 2 0 4 46.22 14.39 1.9640 0 0 4 2 47.60 1.07 1.9103 2 2 1 8 51.29 7.93 1.7812 1 3 0 4 51.94 11.62 1.7605 2 2 2 8 52.03 10.08 1.7576 1 1 4 8 52.52 4.24 1.7424 3 1 0 4 52.69 1.94 1.7371 1 3 1 8 56.75 17.44 1.6222 1 3 2 8 57.12 10.85 1.6125 0 2 4 4 57.70 10.41 1.5978 2 0 4 4 57.90 23.02 1.5927 3 1 2 8 66.17 2.92 1.4122 0 4 0 2 67.33 12.81 1.3907 2 2 4 8 68.27 2.84 1.3738 4 0 0 2 70.92 2.56 1.3289 0 4 2 4 71.51 4.95 1.3194 1 3 4 8 71.91 1.35 1.3129 3 3 0 4 72.52 2.85 1.3034 3 1 4 8 72.95 1.95 1.2968 4 0 2 4 75.73 2.89 1.2560 2 4 0 4 76.50 6.00 1.2452 3 3 2 8 76.70 7.47 1.2425 1 1 6 8 77.22 3.11 1.2354 4 2 0 4 80.24 3.24 1.1963 2 4 2 8 80.93 1.13 1.1879 0 2 6 4 81.42 1.11 1.1820 2 0 6 4 81.71 2.73 1.1785 4 2 2 8 84.50 2.58 1.1465 0 4 4 4 86.44 2.74 1.1257 4 0 4 4 88.32 1.67 1.1066 1 5 0 4 89.87 2.03 1.0915 3 3 4 8 89.99 1.63 1.0904 2 2 6 8 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.