Antimony Schiferl D, Barrett CS Journal of Applied Crystallography 2 (1969) 30-36 The crystal structure of arsenic at 4.2, 78 and 299 K Sample: T = 299 K _database_code_amcsd 0012838 CELL PARAMETERS: 4.3084 4.3084 11.2740 90.000 90.000 120.000 SPACE GROUP: R-3m X-RAY WAVELENGTH: 1.541838 Cell Volume: 181.234 Density (g/cm3): 6.693 MAX. ABS. INTENSITY / VOLUME**2: 334.6850584 RIR: 16.283 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 23.68 5.39 3.7580 0 0 3 2 25.14 1.59 3.5422 1 0 1 6 28.69 100.00 3.1113 0 1 2 6 40.09 33.66 2.2490 1 0 4 6 41.94 35.03 2.1542 1 1 0 6 47.09 5.97 1.9298 0 1 5 6 48.45 4.88 1.8790 0 0 6 2 48.72 4.08 1.8689 1 1 3 12 51.61 17.24 1.7711 2 0 2 6 59.41 9.34 1.5557 0 2 4 6 62.85 4.05 1.4787 1 0 7 6 64.87 2.02 1.4374 2 0 5 6 65.97 10.24 1.4160 1 1 6 12 68.60 12.98 1.3681 1 2 2 12 71.57 2.67 1.3184 0 1 8 6 75.36 8.26 1.2612 2 1 4 12 75.97 1.03 1.2527 0 0 9 2 76.61 4.67 1.2437 3 0 0 6 78.45 1.91 1.2191 0 2 7 6 80.30 1.98 1.1957 1 2 5 12 86.56 1.47 1.1245 2 0 8 6 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.