Eskolaite Finger L W, Hazen R M Journal of Applied Physics 51 (1980) 5362-5367 Crystal structure and isothermal compression of Fe2O3, Cr2O3, and V2O3 to 50 kbars Locality: synthetic Note: P = 0.001 kbar _database_code_amcsd 0017737 CELL PARAMETERS: 4.9510 4.9510 13.5656 90.000 90.000 120.000 SPACE GROUP: R-3c X-RAY WAVELENGTH: 1.541838 Cell Volume: 287.975 Density (g/cm3): 5.258 MAX. ABS. INTENSITY / VOLUME**2: 39.30971384 RIR: 2.434 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 24.56 68.71 3.6243 0 1 2 6 33.70 100.00 2.6599 1 0 4 6 36.29 93.12 2.4755 1 1 0 6 39.87 6.41 2.2609 0 0 6 2 41.59 28.34 2.1714 1 1 3 12 44.31 5.52 2.0442 2 0 2 6 50.35 39.01 1.8121 0 2 4 6 55.00 88.93 1.6694 1 1 6 12 58.54 1.82 1.5769 0 1 8 6 58.56 5.92 1.5762 1 2 2 12 63.64 30.97 1.4622 2 1 4 12 65.28 39.81 1.4292 3 0 0 6 73.18 15.59 1.2934 1 0 10 6 73.57 2.81 1.2874 1 1 9 12 77.05 2.89 1.2378 2 2 0 6 79.30 3.18 1.2081 0 3 6 6 79.30 3.18 1.2081 3 0 6 6 82.32 1.21 1.1713 3 1 2 12 84.52 8.10 1.1463 0 2 10 6 85.99 2.05 1.1305 0 0 12 2 86.78 2.80 1.1222 1 3 4 12 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.