Tenorite Calos N J, Forrester J S, Schaffer G B Journal of Solid State Chemistry 122 (1996) 273-280 A crystallographic contribution to the mechanism of a mechanically induced solid state reaction Note: milling time = 36 min Locality: synthetic _database_code_amcsd 0018819 CELL PARAMETERS: 4.6791 3.4805 5.1183 90.000 98.598 90.000 SPACE GROUP: C2/c X-RAY WAVELENGTH: 1.541838 Cell Volume: 82.418 Density (g/cm3): 6.410 MAX. ABS. INTENSITY / VOLUME**2: 82.18597777 RIR: 4.175 RIR based on corundum from Acta Crystallographica A38 (1982) 733-739 2-THETA INTENSITY D-SPACING H K L Multiplicity 32.18 4.75 2.7813 1 1 0 4 35.40 100.00 2.5356 -1 1 1 4 35.48 37.67 2.5304 0 0 2 2 38.30 96.36 2.3500 1 1 1 4 38.93 29.51 2.3133 2 0 0 2 49.24 24.26 1.8507 -2 0 2 2 52.59 12.81 1.7402 0 2 0 2 57.89 12.91 1.5929 2 0 2 2 61.69 17.96 1.5035 -1 1 3 4 65.05 15.73 1.4339 0 2 2 4 66.35 13.55 1.4089 -3 1 1 4 67.33 13.69 1.3907 2 2 0 4 67.47 11.75 1.3881 1 1 3 4 71.93 9.28 1.3126 3 1 1 4 74.90 7.58 1.2678 -2 2 2 4 75.08 4.52 1.2652 0 0 4 2 80.98 2.87 1.1873 -2 0 4 2 82.01 5.60 1.1750 2 2 2 4 83.05 5.61 1.1629 -3 1 3 4 83.60 3.03 1.1566 4 0 0 2 87.29 2.29 1.1170 -4 0 2 2 88.27 4.98 1.1071 -1 3 1 4 ================================================================================ XPOW Copyright 1993 Bob Downs, Ranjini Swaminathan and Kurt Bartelmehs For reference, see Downs et al. (1993) American Mineralogist 78, 1104-1107.